Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 7.36e+13 ohm | 7.36e+13 ohm | IEC 60093 |
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by .. |