Electrical Properties Metric English Comments
Surface Resistance 7.20e+15 ohm
7.20e+15 ohm
ASTM D257
Arkema Group Orgalloy® RS 6620 Polyamide 6.6 Alloy 20% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group