Polymer Property : Surface Resistance = 7.00e+12 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 7.00e+12 ohm
7.00e+12 ohm
ASTM D257
Rogers Corporation Poron® 4701-50-15 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..
Surface Resistance 7.00e+12 ohm
7.00e+12 ohm
ASTM D257
Rogers Corporation Poron® 4701-50-30 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4..
Surface Resistance 7.00e+12 ohm
7.00e+12 ohm
IEC 93
Vyncolit X6952 Novolac Phenolic
Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn..
Surface Resistance 7.00e+12 ohm
7.00e+12 ohm
IEC 60093
Polyplastics Duranex® CA7200NX Polybutylene Terephthalate (PBT), Antistatic
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Surface Resistance 7.00e+12 ohm
7.00e+12 ohm
ASTM D257
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..