Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 69000 ohm | 69000 ohm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv.. |