Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 610 ohm | 610 ohm | |
Lord Adhesives Aeroglaze® L300 Conductive, Flexible Coating Features and BenefitsDurability - resists abrasion and last for years.Environmental Resistance - resists attack from oils, solvents and chemicals.Versatility - offers flexibility, conductivity and a.. |