Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 600000 ohm | 600000 ohm | |
LATI Latistat 66-06 G/30 PA66, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |