Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 6.31e+8 ohm | 6.31e+8 ohm | ASTM D257 |
Tipco Tipcolite® TG 615 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |