Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 6.10e+13 ohm | 6.10e+13 ohm | 50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology only from DuPont it provides exceptional welding resistanceInformation .. |