Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+9 - 6.02e+16 ohm | 1.00e+9 - 6.02e+16 ohm | Average value: 2.89e+15 ohm Grade Count:50 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |