Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 6.02e+16 ohm | 6.02e+16 ohm | ASTM D257 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |