Polymer Property : Surface Resistance = 500000 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 500000 ohm
500000 ohm
LATI Laticonther 88/10 GR/50 PEEK, 50% Graphite Reinforced
High thermal conductivity product based on Polyetheretherketone (PEEK). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..