Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 5.50e+12 ohm | 5.50e+12 ohm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |