Polymer Property : Surface Resistance = 4.90e+12 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 4.90e+12 ohm
4.90e+12 ohm
ASTM D257
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer
Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and..
Surface Resistance 4.90e+12 ohm
4.90e+12 ohm
ASTM D257
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser..