Polymer Property : Surface Resistance = 4.80e+10 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 4.80e+10 ohm
4.80e+10 ohm
Moisture Resistance; MIL-I-46058C
Humiseal 1A20 Urethane Conformal Coating
Humiseal 1A20 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL..
Surface Resistance 4.80e+10 ohm
4.80e+10 ohm
Moisture Resistance; MIL-I-46058C
Humiseal 1A20LSE Urethane Conformal Coating
Humiseal 1A20LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval pendingPasses ther..
Surface Resistance 4.80e+10 ohm
4.80e+10 ohm
Moisture Resistance; MIL-I-46058C
Humiseal 2A64 Urethane Conformal Coating
Humiseal 2A64 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-46058C)F..