Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 4.42e+14 ohm | 4.42e+14 ohm | Condition A; IPC TM-650 2.5.17.1 |
Arlon 25N Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |