Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 4.20e+16 ohm | 4.20e+16 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Surface Resistance | 4.20e+16 ohm | 4.20e+16 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Asia Pacific) Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Surface Resistance | 4.20e+16 ohm | 4.20e+16 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Europe-Africa-Middle East) Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Surface Resistance | 4.20e+16 ohm | 4.20e+16 ohm | |
Loctite® 3533 Low viscosity fill encapsulant Fill Encapsulant COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |