Surface Resistance 1.00e+13 - 4.00e+16 ohm
1.00e+13 - 4.00e+16 ohm
Average value: 5.09e+15 ohm Grade Count:13
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..