Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 300 ohm | 300 ohm | |
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Surface Resistance | 300 ohm | 300 ohm | |
LATI Larton K/30 PPS, 30% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Surface Resistance | 300 ohm | 300 ohm | |
LATI Latishield 87/28-10A PC, Steel Fiber Reinforced EMI shielding product based on Polycarbonate (PC). Steel fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |