Polymer Property : Surface Resistance = 3.70e+14 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 3.70e+14 ohm
3.70e+14 ohm
Resin Technology Group UV CC-2004 Multi-Functional, UV Curing, Conformal-Coating
Multi-functional UV-CC 2004 is a single component, solvent-less conformal-coating specifically formulated for rapid room temperature cure when exposed to UV light. Thin layer coatings cure almost in..
Surface Resistance 3.70e+14 ohm
3.70e+14 ohm
IEC 60093
Lucobit Lucofin® 7410 HFFR EBA MDH Cable Sheathing
Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and..
Surface Resistance 3.70e+14 ohm
3.70e+14 ohm
E24/125; IPC TM-650 2.5.17.1
Arlon 35N Fast Cure Polyimide Laminate and Prepreg
High reliability and high temperature material35N is a pure polyimide laminate and prepreg system for applications requiring high temperature performance. High Tg results in low Z-direction expansi..