Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.54e+15 ohm | 3.54e+15 ohm | ASTM D257 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Surface Resistance | 3.54e+15 ohm | 3.54e+15 ohm | ASTM D257 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Asia Pacific) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Surface Resistance | 3.54e+15 ohm | 3.54e+15 ohm | ASTM D257 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Europe-Africa-Middle East) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |