Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 10.0 - 3.10e+15 ohm | 10.0 - 3.10e+15 ohm | Average value: 3.01e+14 ohm Grade Count:17 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |