Polymer Property : Surface Resistance = 3.00e+7 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 3.00e+7 ohm
3.00e+7 ohm
LATI Latiohm 73/23-10 CNT POM
Semiconductive/dissipative product based on Polyoxymethylene (POM). Carbon nanotubes.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La..
Surface Resistance 3.00e+7 ohm
3.00e+7 ohm
LATI Latiohm 66-10 H2 CNT G/35 PA66, 35% Glass Fiber Reinforced, Heat Stabilized
Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..