Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.00e+6 ohm | 3.00e+6 ohm | ASTM D257 |
Teknor Apex Telcar® TL-1477B AUTO UV BLACK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Surface Resistance | 3.00e+6 ohm | 3.00e+6 ohm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |
|||
Surface Resistance | 3.00e+6 ohm | 3.00e+6 ohm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |