Polymer Property : Surface Resistance = 2.90e+13 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 2.90e+13 ohm
2.90e+13 ohm
C96/35/90; IPC TM-650 2.5.17.1
Arlon 49N Multifunctional Epoxy Low-Flow Prepreg
49N is a low-flow epoxy prepreg engineered for bonding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. With a high Tg, the prepreg can be used in high-performance or high-te..
Surface Resistance 2.90e+13 ohm
2.90e+13 ohm
C96/35/90; IPC TM-650 2.5.17.1
Arlon 51N Lead-Free Compatible Epoxy Low-Flow
51N is a non-DICY multifunctional epoxy low-flow prepreg system designed to provide high reliability through lead-free solder operations. The high decomposition temperature and high thermal stabili..
Surface Resistance 2.90e+13 ohm
2.90e+13 ohm
E24/125; IPC TM-650 2.5.17.1
Arlon 45N Multifunctional Epoxy Laminate and Prepreg
Arlon 45N is a tough, high Tg (175°C by DSC) multifunctional epoxy laminate and prepreg system designed for use in a variety of higher layer count MLBs. Processable using conventional FR-4 conditi..
Surface Resistance 2.90e+13 ohm
2.90e+13 ohm
E24/125; IPC TM-650 2.5.17.1
Arlon 44N Multifunctional Microdispersed Ceramic Filled Epoxy-Fiberglass Prepreg
Arlon 44N is a high resin content multifunctional (175°C) epoxy prepreg system with a proprietary microdispersed ceramic filler system. 44N is engineered for the filling of clearance holes in thi..