Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.80e+12 ohm | 2.80e+12 ohm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico.. |