Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 1e+8 ohm | <= 1e+8 ohm | ASTM D257-93 |
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing Processed by selective laser sintering (SLS). Windform® SP is a deep black composite polyamide that is a “Top” level material within the polyamide Windform® materials for additive manufacturing.. |
|||
Surface Resistance | <= 1e+8 ohm | <= 1e+8 ohm | ASTM D257-93 |
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite Processed by selective laser sintering (SLS). Windform® XT 2.0 is the evolution of the ground breaking high performance Windform® XT, the carbon fiber reinforced composite material, known for its.. |