Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1e+15 ohm | 1e+15 ohm | IEC 60093 |
Polyram RamSter PF340S4 PBT, 20% Glass Beads 20% Glass bead reinforced PBT for injection molding applications.Information provided by Polyram Ram On Ind. |