Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 178000 ohm | 178000 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics LNP THERMOCOMP RC003 PA 66 (Europe-Africa-Middle East) 15% carbon fibre reinforced Polyamide 66 injection moulding resin. |
|||
Surface Resistance | 178000 ohm | 178000 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics LNP THERMOCOMP RC003SXS PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC003SXS is a compound based on PA 66 resin containing Carbon fiber. Added features include: Electrically Conductive, Heat Stabilized |
|||
Surface Resistance | 178000 ohm | 178000 ohm | ROA; IEC 60093 |
Eurostar Staramide ACF3 PA66, 15% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 15% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Surface Resistance | 178000 ohm | 178000 ohm | ROA; IEC 60093 |
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |