Electrical Properties Metric English Comments
Surface Resistance 1500 ohm
1500 ohm
LATI Latiohm 66-07 PD08 G/30 PA66, 30% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..