Polymer Property : Surface Resistance = 1.60e+17 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 1.60e+17 ohm
1.60e+17 ohm
ASTM D 257
SABIC Innovative Plastics Ultem DT1800E PEI Blend
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re..
Surface Resistance 1.60e+17 ohm
1.60e+17 ohm
ASTM D 257
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Asia Pacific)
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi..
Surface Resistance 1.60e+17 ohm
1.60e+17 ohm
ASTM D 257
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Europe-Africa-Middle East)
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri..
Surface Resistance 1.60e+17 ohm
1.60e+17 ohm
ASTM D257
SABIC Innovative Plastics ULTEM EXUM0167 PEI Blend
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.
Surface Resistance 1.60e+17 ohm
1.60e+17 ohm
ASTM D257
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.
Surface Resistance 1.60e+17 ohm
1.60e+17 ohm
ASTM D257
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend (Asia Pacific)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.
Surface Resistance 1.60e+17 ohm
1.60e+17 ohm
ASTM D 257
SABIC Innovative Plastics Ultem EXUM0169 PEI Blend (Europe-Africa-Middle East)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri..