Polymer Property : Surface Resistance = 1.30e+8 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 1.30e+8 ohm
1.30e+8 ohm
ASTM D257
PolyOne Elastamax XL 0233-1 Polyurethane Compound  (discontinued **)
This is a static dissipative thermoplastic polyurethane compound for injection molding and extrusion applications. Physical Form: Pellet. Standard Color: Black/grey.Information provided by M. A. H..