Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.30e+16 ohm | 1.30e+16 ohm | ASTM D 257 |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |