Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.2e+10 - 1.0e+11 ohm | 3.2e+10 - 1.0e+11 ohm | IS 3396-1979 |
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric .. |