Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 0.38 ohm | 0.38 ohm | |
Parker Chomerics PREMIERâ„¢ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |