Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 0.00700 - 0.0170 ohm @Temperature 35.0 - 121 °C |
0.00700 - 0.0170 ohm @Temperature 95.0 - 250 °F |
Average value: 0.0105 ohm Grade Count:5 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |
|||
Surface Resistance | 0.00700 - 0.0170 ohm @Time 605000 - 7.88e+6 sec |
0.00700 - 0.0170 ohm @Time 168 - 2190 hour |
Average value: 0.0105 ohm Grade Count:5 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |