Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 350 - 400 ohm @Thickness 0.0250 mm |
350 - 400 ohm @Thickness 0.000984 in |
Printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox |
Gwent Electronic Materials C2080529D7 Carbon Flexographic Ink Carbon conductor ink specifically designed for printing on to polymeric or paper substrates using flexographic printing. Ink can be printed at speeds up to 20m/min, with good line definition and go.. |