Polymer Property : Surface Resistivity per Square = 0.070 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.070 - 0.077 ohm

@Thickness 0.0100 mm
0.070 - 0.077 ohm

@Thickness 0.000394 in
Using a 230 stainless steel mesh screen
Gwent Electronic Materials C2110817D5 Conductive Silver Polymer Paste
This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electro-chemical sensors and conductive tracks. It may b..