Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 0.025 - 0.035 ohm @Thickness 0.0100 mm |
0.025 - 0.035 ohm @Thickness 0.000394 in |
Printed onto 125 µm PET film |
Gwent Electronic Materials C2081126P2 Conductive Silver Polymer Paste This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electrochemical sensors and conductive tracks. It may be .. |
|||
Surface Resistivity per Square | 0.025 - 0.035 ohm @Thickness 0.0250 mm |
0.025 - 0.035 ohm @Thickness 0.000984 in |
Using a 230 stainless steel mesh screen |
Gwent Electronic Materials C2110817D5 Conductive Silver Polymer Paste This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electro-chemical sensors and conductive tracks. It may b.. |
|||
Surface Resistivity per Square | 0.025 - 0.030 ohm @Thickness 0.0250 mm |
0.025 - 0.030 ohm @Thickness 0.000984 in |
printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox |
Gwent Electronic Materials C2080815P1 Silver Flexographic Ink Silver conductor ink specifically designed for printing on to polymeric or paper substrates using flexographic printing. Ink can be printed at speeds up to 20m/min, with good line definition and go.. |