Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Breakdown >= 6250 V

@Thickness 0.250 mm
>= 6250 V

@Thickness 0.00984 in
DIN EN 60243
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance)
Rubalit® 708 HP (High Performance) has been developed from Rubalit® 708S. This material shares the same chemical composition, is produced on the same plant and using the identical production techn..