Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | >= 25000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 25000 V @Temperature 194 °F, Time 0.00556 hour |
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF CC 21 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and electrical applications. Fine weave (>30 threads per cm).Information provided by Hippe. |
|||
Dielectric Breakdown | >= 25000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 25000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF CC 21 Woven Cotton Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and electrical applications. Fine weave (>30 threads per cm).Information provided by Hippe. |
|||
Dielectric Breakdown | >= 25000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 25000 V @Temperature 194 °F, Time 0.00556 hour |
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF CP 23 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and low-voltage electrical applications. Good electrical properties when exposed to normal and high relative humidity.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 25000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 25000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF CP 23 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical and low-voltage electrical applications. Good electrical properties when exposed to normal and high relative humidity.Information provided by Hippe. |