Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 11000 V @Thickness 1.57 mm |
11000 V @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S/S |
Industrial Laminates/Norplex NP193M Synthetic Fabric Base Grade Description: 17 oz. aramide and “soft glass†fibers are combined to make a fabric that is stronger than pure aramide and less abrasive than glass fabrics. This material is impregnated with.. |