Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 9.70e+15 ohm-cm | 9.70e+15 ohm-cm | Tinfoil Electrodes; ASTM D257 |
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Dry as Extruded Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Electrical Resistivity | 9.70e+15 ohm-cm | 9.70e+15 ohm-cm | ASTM D257 |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |