Polymer Property : Electrical Resistivity = 8333 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 8333 ohm-cm
8333 ohm-cm
Nabaltec ACTILOX® B20 AlO(OH) Boehmite
Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature stabilitySynergistic effects with other flame retardantsHigh acid resistance..
Electrical Resistivity 8333 ohm-cm
8333 ohm-cm
Nabaltec APYRAL® AOH 20 AlO(OH) Boehmite
Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature applicationsLow sedimentation at good viscosity performance in resinsGood ch..