Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 7.74e+13 ohm-cm | 7.74e+13 ohm-cm | |
Arkema Group Pebax® 7233 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 72 shore D Highest modulus PEBAX Applications: medical, extrusion SportISO data provided by the manufacturer, Arkema. |