Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+12 - 7.00e+16 ohm-cm | 1.00e+12 - 7.00e+16 ohm-cm | Average value: 2.56e+16 ohm-cm Grade Count:9 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |