Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 6000 ohm-cm | 6000 ohm-cm | Average |
Shakespeare Sanstat® CN125 .52mm Nylon 66 Monofilament Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by .. |