Polymer Property : Electrical Resistivity = 6.70e+15 ohm-cm
Polymer Property :
Electrical Resistivity =
6.70e+15 ohm-cm
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Electrical Resistivity
6.70e+15
ohm-cm
6.70e+15
ohm-cm
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled
Crystalline Polymer Blend, Glass Filled, Impact Modified