Polymer Property : Electrical Resistivity = 6.00e+13 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 6.00e+13 ohm-cm
6.00e+13 ohm-cm
ASTM D257
Toyobo Pelprene™ P-70B Polyester TPE
Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block..