Polymer Property : Electrical Resistivity = 5.00e+17 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.00500 - 5.00e+17 ohm-cm
0.00500 - 5.00e+17 ohm-cm
Average value: 4.06e+16 ohm-cm Grade Count:53
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..