Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 4.63e+16 ohm-cm | 4.63e+16 ohm-cm | ASTM D257 |
Plenco 50240 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.. |